1、 2Cr13 TP420

 


Chemical composition:

C :0.16~0.25
Si:≤1.00
Mn:≤1.00
S :≤0.030
P :≤0.035
Cr:12.00~14.00
Ni:May contain≤0.60

Mechanical Properties:

Tensile strength σb (MPa):Quenching and tempering,≥635
Conditions yield strength σ0.2 (MPa):Quenching and tempering,≥440
Elongation δ5 (%):Quenching and tempering,≥20
Section shrinkage ψ (%):Quenching and tempering,≥50
Impact Energy Akv (J):Quenching and tempering,≥63
hardness :Annealing,≤223HB;Quenching and tempering,≥192HB
1.Heat treatment and microstructure specifications :
Heat treatment specifications :1)Annealing,800~900℃Slow cooling or rapid cooling at about 750 ℃; 2) quenching, 920 ~ 980 ℃ oil
Cold; 3) Tempering, 600 ~ 750 ℃ fast-cooling.
Microstructure: Organizing for the martensitic 。
2.Delivery status: generally heat treatment delivery, the treatment types specified in the contract; not indicated, according to the delivery without heat treatment 。

2、

High-temperature alloy such as Monel Monel400, Hastelloy incoloy600 Department, 800 Series, etc. 。

3、

Nuclear grade stainless steel, such as nuclear power boiler super TP30432 pipe and tube
 
Copright @ 2010 ZHEJIANG YONGSHANG STAINLESS INDUSTRIAL CO.LTD All Rights Support by: brightcn.com